Internal friction in Invar Fe-35 % Ni alloy after combined SPD by hydroextrusion and drawing
Vernadsky National Library of Ukraine
Переглянути архів ІнформаціяПоле | Співвідношення | |
Title |
Internal friction in Invar Fe-35 % Ni alloy after combined SPD by hydroextrusion and drawing
|
|
Creator |
Nadutov, V.M.
Vashchuk, D.L. Pilipenko, A.N. Davidenko, O.A. Beloshenko, V.A. |
|
Subject |
Characterization and properties
|
|
Description |
The temperature dependence of internal friction on frequency of ~3 Hz and ~60 Hz were studied in Invar Fe-35.0% Ni-0.49% Mn-0.03%C alloy after annealing at 1373 K and combined severe plastic deformation (SPD) by hydroextrusion and subsequent drawing with the total degree of accumulated deformation ε Σ = 4.69. The reduction of the relaxation IF peak intensity is observed in deformed sample of the alloy at ~380 K (the activation energy 0.82-0.93 eV) due to decreasing of mechanical and magnetomechanical relaxation losses the contribution of which is renewed after ageing of the deformed alloy. The damping growth nearby temperatures 780-820 K after combined SPD and partial its reduction after ageing of the alloy were revealed. The estimated activation energy of the relaxation process is 1.82-1.97 eV.
|
|
Date |
2017-06-12T07:13:21Z
2017-06-12T07:13:21Z 2014 |
|
Type |
Article
|
|
Identifier |
Internal friction in Invar Fe-35 % Ni alloy after combined SPD by hydroextrusion and drawing / V.M. Nadutov, D.L. Vashchuk, A.N. Pilipenko, O.A. Davidenko, V.A. Beloshenko // Functional Materials. — 2014. — Т. 21, № 1. — С. 52-58. — Бібліогр.: 22 назв. — англ.
1027-5495 DOI: dx.doi.org/10.15407/fm21.01.052 http://dspace.nbuv.gov.ua/handle/123456789/120401 |
|
Language |
en
|
|
Relation |
Functional Materials
|
|
Publisher |
НТК «Інститут монокристалів» НАН України
|
|